Hi there,
There is an issue with role permissions that is being worked on at the moment.
If you are having trouble with access or permissions on regional forums please post here to get access: https://www.boards.ie/discussion/2058365403/you-do-not-have-permission-for-that#latest

Underfloor heating and drying out slab

  • 23-06-2011 9:29am
    #1
    Registered Users, Registered Users 2 Posts: 24


    Just turned on my underfloor heating and will be gradually increasing the temperature to dry the slab out. What is the highest temperature which I should bring the slab up to during this process?


Comments

  • Registered Users, Registered Users 2 Posts: 5,965 ✭✭✭creedp


    Dugsy wrote: »
    Just turned on my underfloor heating and will be gradually increasing the temperature to dry the slab out. What is the highest temperature which I should bring the slab up to during this process?

    I'd be interested in this as well as its been 3 weeks since I poured the screeds and now plan to turn on the the UFH to assist with drying out process upstairs at least. I had hoped to be able to allow them the dry out naturally but would need a least 3 months for this. Given that there was a 6 week delay in getting them poured and the fact that I have to move into house in Sept I need to accelerate the process if at all possible. I was hoping to start with an UFH temp of 20c and increase to 35c over a 2 week period. Would this be too severe?

    For downstairs I have a polished concrete finish and won't turn on UFH for at least 6 weeks and then gradually bring the temp up to 35c over a period of 4 weeks as I am worried about hairline cracks developing in screed. Not as problematic here as the floors will not be covered so they can continue to dry out over time.

    Bty I asked this before but I'll do so again, how can I measure the moisture content of the screeds so that I can plan when to start the joinery/tile work? I don't necessarily want to purchase an expensive meter which I will never again use and I'm assuming the inexpensive ones are of little value.

    Thanks


  • Registered Users, Registered Users 2 Posts: 155 ✭✭peterc14


    I have 75mm sand/cement screed with UFH and this is the program I am following..

    . Screed Poured
    . Leaving to dry naturally for 6 weeks
    . UFH turned on at 25 deg for 3 days
    . Then up by 5 deg each day until max
    . Max Temp for 4 days
    . Heating off and floor allowed to cool (4/5 days)
    . Start Tiling
    . No heat back on until 4 weeks after tiling completed

    From reading different opinions this is the way I decided to go about things. I am sure people will have differing opinions.